Beyond a Decoration; Mineralogical and Micro-structural Study of the Early Bronze Age “Life Cycle Jar” from Keshik Cemetery, Sistan and Balouchistan, Iran
Bibliographic Data
| ID | 12940540 |
|---|---|
| Authors | Yasin Sedghi (corresponding author), Farahangiz Sabouhi Sani (Isfahan University of Art), N Eskandari (0000-0001-8461-9000, University of Tehran), Mohammadamin Emami (0000-0002-7484-1991, Université Bordeaux Montaigne) |
| Year | 2022 |
| Volume | 13 |
| Issue | 2 |
| Pages | 117-128 |
| Publication date | 2022-11-02 |
| Peer Reviewed | Yes |
| Open Access | Yes |
| Type | ARTICLE |
| Venue | Interdisciplinaria Archaeologica - Natural Sciences in Archaeology (JOURNAL) |
| Journal identifiers | ISSN: 1804-848X • E-ISSN: 2336-1220 |
| Publisher | Archeologické centrum Olomouc (PUBLISHER • CZ) |
| DOI | 10.24916/iansa.2022.2.2 |
| OpenAlex | W4307989781 |
| Language | EN |
| Citations received | 1 |
| References cited | 19 |
The present study focuses on a unique pottery vessel, the so-called “Life Cycle Jar”, and nine other potsherds which were discovered in the Keshik cemetery, Baluchistan, south-east Iran. Samples were investigated through classical analytical methods such as thin-section petrography, X-ray powder diffraction (XRPD), and scanning electron microscopy coupled with energy dispersive X-ray fluorescence (SEM-EDX) to determine the production techniques, fabric characterisation, as well as the pigments applied to decorate the surface of the Life Cycle Jar. Mineralogical and chemical investigations revealed that the pottery pieces were similar in raw materials, and produced locally. Samples show a wheel-thrown signature based on the definite orientation of pores and structural character in their thin sections. The potter pieces were fired under oxidation processes demonstrated by the red and green colour of the matrix. The investigated pottery samples were defined as high-fired sherds (ca. 800–950°C), due to the presence of inclusions in the form of reacted calcite in rhombohedra crystal structure, and hematite within the matrix of the pottery. The microstructural characteristics of the pottery pieces showed that the manufacturing temperature was no higher than 950 °C, by presintering texture. The investigations on the painted decoration on the Life Cycle Jar suggested that iron oxide and manganese oxide was used as the colourant agent in the decoration
Archaeology · Calcite · Composite material · Geography · Hematite · JAR · Manganese · Metallurgy · Mineralogy · Petrography · Pottery · Scanning electron microscope · Texture (cosmology · Building materials and conservation · Chemistry · Conservation Techniques and Studies · Cultural Heritage Materials Analysis · Materials Science
Ceramic composition at Chalcolithic Shiqmim, northern Negev desert, Israel
An approach to the dynamics of clay firing
The presence of calcite in archeological ceramics
Influence of firing conditions on ceramic products
Heated goethite and natural hematite
Temperature evolution inside a pot during experimental surface (bonfire) firing
Investigating ceramic production during the Proto-Elamite period at Tepe Yahya, southeastern Iran
Grog, Petrology, and Early Transcaucasians at Godin Tepe
Sistan and Baluchistan Project
Preliminary Report on the Survey of Hajjiabad-Varamin, a Site of the Konar Sandal Settlement Network (Jiroft, Kerman, Iran)
Technological examination of Neolithic-Bronze Age pottery from central and southeast Europe and from the Near East
Sistan and Baluchistan Project
Effects of Temper on Strength of Ceramics
A surface collection at Chegerdak, a Bronze Age centre in the Jazmurian basin (South-Eastern Iran)
Ceramic technology
Ceramic abandonment. How to recognise post-depositional transformations
Ceramic technology
Ceramic technology. How to reconstruct the firing process
Infrared spectroscopy in the mineralogical characterization of ancient pottery
| Citation velocity | historical |
|---|---|
| Highly cited | No |