Skip to main content

ETHNOS_APP

Home • Search • Journals • List 0

Effect of CAD/CAM Ceramic Thickness on Shade Masking Ability of Discolored Teeth

In Vitro Study

Bibliographic Data

ID15464321
AuthorsPassent Ellakany (0000-0002-2995-8111, Imam Abdulrahman Bin Faisal University, corresponding author), Marwa Madi (0000-0002-3014-0405, Imam Abdulrahman Bin Faisal University), Nourhan M Aly (0000-0002-8729-2485, Alexandria University), Zainb S Al-Aql (King Abdulaziz Medical City), Maher AlGhamdi (Imam Abdulrahman Bin Faisal University), Abdulrahman Aljeraisy (Imam Abdulrahman Bin Faisal University), Adel S Alagl (0000-0001-6274-7677, Imam Abdulrahman Bin Faisal University)
Year2021
Volume18
Issue24
Pages13359-13359
Publication date2021-12-18
Peer ReviewedYes
Open AccessYes
TypeARTICLE
VenueInternational Journal of Environmental Research and Public Health (JOURNAL)
Journal identifiersISSN: 1661-7827 • E-ISSN: 1660-4601
PublisherMultidisciplinary Digital Publishing Institute (PUBLISHER • CH)
DOI10.3390/ijerph182413359
PMID34948965
OpenAlexW4200378299
LanguageEN
References cited42

Shade matching is a common challenge that dentists face during fabrication of esthetic dental restoration. Thus, the aim of the current study was to assess the masking ability of two types of CAD/CAM ceramics for gaining high esthetic prosthesis. This in vitro study used a total sample size of 66 lithium disilicate (LD) and leucite reinforced (LR) CAD/CAM ceramics sub-grouped into three thicknesses: 0.5, 1, and 1.5 mm. Nine shades of natural dentin die materials were prepared as a replica of the underlying tooth structure. The difference in color (ΔE) and translucency parameter (TP) were assessed for both tested ceramics at the three thicknesses. One-way ANOVA was performed to compare the three thicknesses of each ceramic, followed by multiple pairwise comparisons between both ceramics. LR had significantly higher ΔE than LD at all thicknesses used unlike the case in TP. Thickness of 0.5 mm exhibited the highest ΔE and TP, while 1.5 mm thickness showed the lowest ΔE and TP in both ceramics. Increase in ceramic thickness had a great impact on both color masking ability of the underlying tooth structure and its translucency. The higher the ceramic thickness, the better the masking ability and the lower the translucency was reported

Ceramic · Color difference · Composite material · Cubic zirconia · Dental ceramics · Dentin · Lithium disilicate · Masking (illustration · Significant difference · Computer Science · Dental Implant Techniques and Outcomes · Dental materials and restorations · Dental Research and COVID-19 · Dentistry · Materials Science · Mathematics · Medicine · Orthodontics